Fender-TTM TPU series (1090T series)
1. UL certified V0 grade polyether TPU:
UL94-V0 (1.5mm) flame retardant grade, fully support the conventional structural cable through the IEC60332-1-2 single vertical burning test;
2. High and low-temperature shrinkage rate, shrinkage rate ≤1% in high and low-temperature cycle test;
3. High security and reliability, support optic cable through various environmental tests and life tests:
Mold resistance
Authoritative certified mold-resistant materials: through the military standard mold resistance test (GJB150.10);
Hydrolysis resistance: Pass 1000/2000Hrs hydrolysis resistance test (different model) (85°C/85% RH, 1000/2000 Hrs);
High and low-temperature resistance: Wide temperature range for use, Pass 720Hrs high-temperature test (125°C, 720Hrs) and low-temperature destructive tests such as low-temperature winding (-50°C) and low-temperature shock (-50°C);
Acid and alkali resistant, oil resistant, chemical resistant: Pass various acid and alkali resistance, oil resistance and chemical resistance test (e.g: acid and alkali resistance: 23°C/168h, intensity change rate ≤ 30%, extended rate ≥100%; oil resistance: 70 °C / 24h oil resistance test, strength, and elongation, change rate ≤ 30%);
UV resistant: Pass UL1581 UV test (720Hrs UV cycle test, strength, and elongation, retention rate ≥ 80%);
4. High wear resistance: Polar material, high cohesive energy, and wear resistance are much better than conventional low-smoke halogen-free polyolefin materials (LSZH).
Technical Data Sheet | Model | ||||
Material Properties | Test Standard | Test Condition | Unit | 2885F-ESU-1088S | |
General Characteristics | Material Category | - | - | - | |
Appearance(Light/Semi-matte/Frosted) | - | - | - | ||
Extrusion/Injection | - | - | - | ||
Physical Characteristics | Hardness | ISO 48 | 15S | Shore A | 85 |
Proportion | ISO 1183 | - | g/cm³ | 0.951 | |
Melt Index | ISO 1133-1:2011 | 190℃/2.16kg | g/10min | 3.2 | |
Brittle Temperature | ISO 812 | - | ℃ | ||
Mechanical Properties | Elongation | ISO37:2017 | 200mm/min | % | 475 |
Tensile Strength | ISO37:2017 | 200mm/min | Mpa | 14.5 | |
Tearing Strength | ISO34-1:2015 | 500mm/min | KN/m | ||
Hot Air Aging | Elongation Retention Rate | ISO37:2017 | - | % | |
Tensile Strength Retention Rate | ISO37:2017 | - | % | ||
Electrical Performance | Volume Resistivity | ASTM D257 | - | Ohm-cm | |
Permittivity | ASTM D150 | - | - | ||
Combustion Performance | Vertical Burning Test | UL 94 | 3.0/6.0mm | - | |
Oxygen Index | ASTM D2863 | - | % | ||
Feature |
· Competitive price · Respond immediately · Strong R&D capability · Excellent after-sales service