1. If the surface of TPR thermoplastic rubber products is strictly required, it must be dried before injection moldingGenerally, it is hopper drying at 70~80℃/2h or tray drying at 80~100℃/1h. For tr...
Ⅰ. Usually thermoplastic rubber elastomers are easier to agglomerate, and the reasons for agglomeration are as follows:1. If the hardness is too low, such as materials close to 0 degrees, it is usual...
Stress-strain characteristics of thermoplastik elastomer (TPE)Stress-strain characteristics are test values used to demonstrate how an elastomer will behave when stretched. There are several common te...